Where possible, increase thickness above the minimum or stiffen the geometry with ribs or fillets.
You do not need to add a shrinkage factor when preparing the file: the printer compensates for it automatically.
For SLA parts in white or black resin, use these reference design values.
If a part is hollow, the liquid resin must be able to get out: use walls of at least 2 mm and a drain hole of at least 3.5 mm in diameter.
After printing, each part goes through these post-processing steps:
1. Wash in isopropyl alcohol (IPA) to remove residual liquid resin.
2. Dry the part completely.
3. Final UV curing in an ultraviolet oven, which gives the part its final hardness and mechanical strength.
4. Manual removal of the supports.
These are design guidelines: final feasibility depends on the geometry, size, material and functional requirements of the part.